Reaction to fire class as per DIN 4102-4: B 2 (corresponds to the european class D-s2,d0) |
Charring rate: 0.7mm/minute |
Differential shrinkage ratio perpendicular to the grain: 0.24 %/per 1% moisture change |
Thermal conductivity λ parallel to the adhesive joints: 0.13 W/(mK) |
Thermal conductivity λ perpendicular to the glue-lines: 0.15 W/(mK) |
Water vapor diffusion resistance factor µ: 40 |
The natural durability and corrosion resistance (resistance to aggressive chemical attacks) of glulam corresponds to the natural durability and corrosion resistance of the respective wood-species, regardless of the adhesive used. |